Guy at the supply shop called my emulsion coats "sloppy" and it stung but helped
I was picking up a quart of emulsion at a shop over in Akron two weeks ago and the guy behind the counter watched me coat a screen on his demo table. He pointed at my squeegee side and just goes "that's sloppy, you're pushing too fast and loading one edge." I was kinda annoyed at first but he showed me how he does two slow passes on the shirt side and one on the ink side, then lets it dry flat for about an hour before flipping it. My last batch of 12 shirts came out way cleaner at the edges, no more thin spots burning through in the wash. Anybody here got a coat count that works better for 110 mesh? I'm still messing with it.