Vent: Tried that new UV-cure sealant on a big storefront job in Denver and it failed hard
Honestly, I followed the spec sheet to the letter on a 20-foot run of insulated units, but after three days in direct sun the sealant turned brittle and started pulling away. Ngl, I'm back to trusting my old polysulfide method for anything over 10 feet, what's your go-to for high UV exposure areas?
2 comments
Log in to join the discussion
Log In2 Comments
veramartin2d ago
Guess the spec sheet forgot to mention Denver sun is basically a free laser show. I mean, three days? That stuff gave up faster than my willpower at a hardware store. Sticking with polysulfide too, it's boring but at least it doesn't quit on you.
6
black.wesley2d ago
Man, that's just how everything is built these days, isn't it?